General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.69 g/cm³ Show Material materials with Density of 8.69 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.47E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.47E-5 1/K |
Coefficient of thermal expansion, transverse | 23.0 °C | 5.6E-3 1/K Show Material materials with Coefficient of thermal expansion, transverse of 5.6E-3 1/K |
Specific heat capacity | 23.0 °C | 399.11 J/(kg·K) Show Material materials with Specific heat capacity of 399.11 J/(kg·K) |
Thermal conductivity | 23.0 °C | 249 W/(m·K) Show Material materials with Thermal conductivity of 249 W/(m·K) |
Thermal conductivity, through-plane | 23.0 °C | 94.14 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 94.14 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 3.47E+7 S/m Show Material materials with Electrical conductivity of 3.47E+7 S/m |
Electrical conductivity, transverse | 23.0 °C | 1.54E+7 S/m Show Material materials with Electrical conductivity, transverse of 1.54E+7 S/m |
Electrical resistivity | 23.0 °C | 2.9E-8 Ω·m Show Material materials with Electrical resistivity of 2.9E-8 Ω·m |
Magnetic
Property | Value |
---|---|
Magnetic properties | magnetic |
Technological properties
Property | ||
---|---|---|
Coating | Different coating layers are available upon request. |