Dichte: 8.27 g/cm³

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Pure/Low Nickel Alloy

Alloy 360 TB00 (N03360)

Geliefert von:

Materion Brush GmbH

Pure/Low Nickel Alloy

Alloy 360 TD01 (N03360)

Geliefert von:

Materion Brush GmbH

Wrought Copper Bronze Aluminium Bronze

EN 12164 Grade CuZn21Si3P R500

Wrought Copper Bronze Aluminium Bronze

EN 12164 Grade CuZn21Si3P R600

Wrought Copper High Copper Alloy

EN 12166 Grade CuBe2Pb R1150

Wrought Copper High Copper Alloy

EN 12166 Grade CuBe2Pb R1300

Wrought Copper High Copper Alloy

EN 12166 Grade CuBe2Pb H350

Pure/Low Nickel Alloy

Alloy 360 TD02 (N03360)

Geliefert von:

Materion Brush GmbH

Pure/Low Nickel Alloy

Alloy 360 TD04 (N03360)

Geliefert von:

Materion Brush GmbH

Wrought Copper Bronze Aluminium Bronze

EN 12164 Grade CuZn21Si3P H130

Wrought Copper Bronze Aluminium Bronze

EN 12164 Grade CuZn21Si3P H110

Wrought Copper Bronze Aluminium Bronze

EN 12164 Grade CuZn21Si3P H150

Wrought Copper Bronze Aluminium Bronze

EN 12165 Grade CuZn21Si3P H110
Seite 1 von 28