High density engineered thermoplastics / reinforced polyamide 12 (PA12) with metal particles

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

4.0 - 11.0 g/cm³

Show Material materials with Density of 4.0 - 11.0 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

0.5 - 11.0 GPa

Show Material materials with Elastic modulus of 0.5 - 11.0 GPa

Elongation

0.5 - 4.0 %

Show Material materials with Elongation of 0.5 - 4.0 %

Impact strength, Charpy notched

5.0 - 6.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.0 - 6.0 kJ/m²

Impact strength, Charpy unnotched

10 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 10 kJ/m²

20 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

Tensile strength

30.0 - 60.0 MPa

Show Material materials with Tensile strength of 30.0 - 60.0 MPa

at 0.5-4% strain

Thermal

PropertyValue

Coefficient of thermal expansion

5.5e-05 - 6.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 5.5e-05 - 6.5e-05 1/K

Thermal conductivity

1.5 - 3.5 W/(m·K)

Show Material materials with Thermal conductivity of 1.5 - 3.5 W/(m·K)

Electrical

PropertyValue

Electrical resistivity

0.1 - 10.0 Ω·m

Show Material materials with Electrical resistivity of 0.1 - 10.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

X-ray equipment, accessories for orthodontics and dentistry, radiopaque catheters, detectable surgical tools, shielding systems

Fillers

Metal Powder

Processing methods

Injection molding