EN 12166 Grade CuZn40Mn1Pb1 H090

Want to keep this datasheet? Save it now in your required format

Description

CuZn40Mn1Pb1 (CW720R former identification: CuZn40MnPb) is an unhardenable copper alloy. High hardness and strength parameter are achievable by cold forming only. Manganes increases corrosion resistance and sliding qualities. Improved machinability by Pb-addition. Processing properties: warm forming: good cold forming: unfavorable machinability: good hard soldering: moderately soft soldering: very good TIG-welding: unfavorable burnishing: very good Application for roller bearing cages and screw machine products.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.1 - 8.3 g/cm³

Show Material materials with Density of 8.1 - 8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

95 GPa

Show Material materials with Elastic modulus of 95 GPa

Hardness, Brinell

20.0 °C

90 - 150 [-]

Show Material materials with Hardness, Brinell of 90 - 150 [-]

Hardness, Vickers

20.0 °C

100 - 135 [-]

Show Material materials with Hardness, Vickers of 100 - 135 [-]

Shear modulus

20.0 °C

36 GPa

Show Material materials with Shear modulus of 36 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

200.0 °C

1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

20.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Thermal conductivity

20.0 °C

67 W/(m·K)

Show Material materials with Thermal conductivity of 67 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

8.70E+6 S/m

Show Material materials with Electrical conductivity of 8.70E+6 S/m

Electrical resistivity

20.0 °C

1.15E-7 Ω·m

Show Material materials with Electrical resistivity of 1.15E-7 Ω·m

Chemical properties

PropertyValue

Aluminium

0.2 %

Show Material materials with Aluminium of 0.2 %

Copper

57 - 59 %

Show Material materials with Copper of 57 - 59 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

1 - 2 %

Show Material materials with Lead of 1 - 2 %

Manganese

0.5 - 1.5 %

Show Material materials with Manganese of 0.5 - 1.5 %

Nickel

0.6 %

Show Material materials with Nickel of 0.6 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Tin

0.3 %

Show Material materials with Tin of 0.3 %