VYPET™ VNT-615 FR

Alternative and trade names
PET-GF15
Want to keep this datasheet? Save it now in your required format

Description

Polyethylene Terephthalate (PET) with 15% Glass Fiber Reinforced and Flame Retardant.

Properties

General

Density

ρ

1.55 g/cm³ at 23 °C

ASTM D792

Mechanical

Flexural modulus

Ebend

5.9 GPa at 23 °C

Show Polyethylene Terephthalate (PET) materials with Flexural modulus of 5.9 GPa at 23 °C

ISO 178, 2 mm/min

Flexural strength

σbend

150 MPa at 23 °C

Show Polyethylene Terephthalate (PET) materials with Flexural strength of 150 MPa at 23 °C

ISO 178, 2 mm/min

Impact strength, Izod notched

IIzod,not

6 kJ/m² at 23 °C

Show Polyethylene Terephthalate (PET) materials with Impact strength, Izod notched of 6 kJ/m² at 23 °C

ISO 180

Tensile strength

Rm

105 MPa at 23 °C

Show Polyethylene Terephthalate (PET) materials with Tensile strength of 105 MPa at 23 °C

ISO 527, 5 mm/min

Thermal

Ash content

cash

15 % at 23 °C

ASTM D5630

Flammability

V0, V0 5VA for 3.2 mm sample UL94

Heat deflection temperature, 1.80 MPa

HDT1.8,MPa

200 °C

ISO 75

Electrical

Dielectric strength

EDS

37 kV/mm at 23 °C

ASTM D149, 1.6 mm, 500V/s in oil

Dissipation factor, 1kHz

ε''1KHz

2E-3 [-] at 23 °C

ASTM D150

Volume resistivity

ρel, vol

1.00E+18 Ω·cm at 23 °C

ASTM D257

Rheological Properties

Shrinkage

cshrink

0.4 % at 23 °C

ASTM D955

Shrinkage, transverse

cshrink, trans

0.9 % at 23 °C

ASTM D955

Technological properties

Application areas

Electrical components, appliances and structral applications.

Color

Black

Filler Type

Fillers

15% Glass Fiber and Mineral Powder

Processing Tag

Processing methods

  • Drying to Dew Point:-18°C or lower
  • Feed zone: 260-270°C
  • Middle zone: 265-275°C
  • Front zone: 270-290°C
  • Nozzle: 275-295°C
  • Melt temperature: 275-295°C
  • Mold temperature (thick wall parts): 95-120°C
  • Mold temperature (thin wall parts): 95-120°C
  • Injection Pressure: 55-85 MPa
  • Injection Speed: Fast
  • Back Pressure: 25-50 psi
  • Screw Speed: 50-75 rpm
  • This material data has been provided by Lavergne.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.