SABIC® LLDPE 320NT

Want to keep this datasheet? Save it now in your required format

Description

SABIC® 320NT is an ethylene-butene copolymer designed for wire and cable application. it is designed for high speed cable extrusion line, product use 320NT has excellent cable outlook, compare to the other polyethylene, 320NT is designed to reduce the use of additive during compounding, suggest the customer to optimize the silane and peroxide amount for 320NT based material, suitable for one-step silane crosslinking low voltage power cable insulation. 320NT contains no slip and no antiblock.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Melting point

120 °C

Show Material materials with Melting point of 120 °C

SABIC method

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.25 [-]

Show Material materials with Dielectric constant of 2.25 [-]

ASTM D150

Dielectric strength

23.0 °C

37 kV/mm

Show Material materials with Dielectric strength of 37 kV/mm

ASTM D150

Dissipation factor

23.0 °C

7E-4 [-]

Show Material materials with Dissipation factor of 7E-4 [-]

ASTM D150

Technological properties

Property
Application areas

Wire & cable