Rilsan® 6189 Yellow Fluid Bed Powder

Rilsan® fluid bed powders are thermoplastic polyamides obtained from renewable resources. Outstanding characteristics: abrasion resistance, corrosion resistance, impact resistance, sound reduction, flexibility, low coefficient of friction.

This material data has been provided by Arkema Technical Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTesting StandardComment

Density

1.18 - 1.23 g/cm³

Show Supplier Material materials with Density of 1.18 - 1.23 g/cm³

ISO 1183

relative density

Mechanical

PropertyValueTesting StandardCondition

Impact energy, coating

160 J

Show Supplier Material materials with Impact energy, coating of 160 J

ASTM D2794

Yield strength

24 MPa

Show Supplier Material materials with Yield strength of 24 MPa

ISO 527-1/-2

cond.

43 MPa

Show Supplier Material materials with Yield strength of 43 MPa

ISO 527-1/-2

dry

Thermal

PropertyValueConditionTesting Standard

Melting point

183 - 193 °C

Show Supplier Material materials with Melting point of 183 - 193 °C

dry

ISO 1218

Electrical

PropertyValueTesting Standard

Dielectric strength

15.7 - 41.3 kV/mm

Show Supplier Material materials with Dielectric strength of 15.7 - 41.3 kV/mm

ASTM D149

Technological properties

Property
Application areas

Powder Coatings - Automotive & Transportation,Powder Coatings - General Purpose,Powder Coatings - Healthcare,Powder Coatings - Wire Goods

Color

Yellow

Covering efficiency

0.35 kg/m²

Covering efficiency, thickness

300 µm