Elastizitätsmodul: 190.8 GPa

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-2 Grade P235GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-2 Grade P265GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel molybdenum Steel

EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-5 Grade S355J2W normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-5 Grade S355K2W normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10225 Grade S420G1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-3 Grade S460N normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-3 Grade S460NL normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S275M thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S275ML thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S355M thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S355ML thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S420M thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S420ML thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S460M thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10025-4 Grade S460ML thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10028-5 Grade P420M thermomechanically rolled

Geliefert von:

2 Matmatch-Lieferanten

Seite 1 von 80