EN 10025-3 Grade S460N normalized or normalized formed (+N)

Want to keep this datasheet? Save it now in your required format

Description

The alloyed, normalised/normalising rolled high grade steel S460N is a weldable fine-grained steel with a min. yield point of 460 N/mm². The steel is applicated in normalized condition for several types of welded constructions such as fixed and movable storage container, high-pressure pipes, bridge and load-bearing constructions etc. Cold forming: Suitability for cold bending, folding, cold flanging or cold welting has to be agreed. For sheet, strip and wide flat steel in normalized condition, for nominal thickness (s) up to 16 mm can be warranted the following bending radius values: longitudinal: 5 x s transverse: 4 x s Sheet and strip of nominal thicknesses < 8 mm for cold forming of sections is available on arrangement (e.g. for production of hollow sections). Requirements regarding hot dip zinc coating by arrangement.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

16 - 17 %

Show Material materials with Elongation of 16 - 17 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

510 - 720 MPa

Show Material materials with Tensile strength of 510 - 720 MPa

Yield strength

20.0 °C

370 - 460 MPa

Show Material materials with Yield strength of 370 - 460 MPa

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.55 - 0.7 %

Show Material materials with Copper of 0.55 - 0.7 %

Manganese

1 - 1.7 %

Show Material materials with Manganese of 1 - 1.7 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

0.8 %

Show Material materials with Nickel of 0.8 %

Niobium

0.05 - 0.2 %

Show Material materials with Niobium of 0.05 - 0.2 %

Nitrogen

0.03 %

Show Material materials with Nitrogen of 0.03 %

Phosphorus

0.03 - 0.04 %

Show Material materials with Phosphorus of 0.03 - 0.04 %

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

Sulfur

0.025 - 0.03 %

Show Material materials with Sulfur of 0.025 - 0.03 %

Titanium

0.03 - 0.05 %

Show Material materials with Titanium of 0.03 - 0.05 %

Vanadium

0.05 - 0.2 %

Show Material materials with Vanadium of 0.05 - 0.2 %