Ferritischer Edelstahl
DIN 17440 Grade X6Cr17 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT2)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT1)Martensitischer Edelstahl
EN 10088-1 Grade X20Cr13 quenched and tempered (+QT700)Martensitischer Edelstahl
EN 10088-1 Grade X30Cr13 quenched and tempered (+QT850)Martensitischer Edelstahl
EN 10088-1 Grade X39Cr13 quenched and tempered (+QT800)Martensitischer Edelstahl
DIN 17440 Grade X15Cr13 quenched and tempered (+QT)Nickel Chromium Alloy
DIN 17742 Grade NiCr20TiAl precipitation hardened (+P)Nickel Chromium Alloy
WL 2.4630 Grade NiCr20Ti soft annealed (+A)Martensitischer Edelstahl
SEW 400 Grade X35CrMo17 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10088-1 Grade X46Cr13 quenched and tempered (+QT850)Ferritischer Edelstahl
DIN 1654-5 Grade X6Cr17 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X30Cr13 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X30Cr13 quenched and tempered (+QT)Ferritischer Edelstahl
DIN 1654-5 Grade X6Cr17 annealed to achieve spheroidized carbides (+AC)Ferritischer Edelstahl
DIN 1654-5 Grade X6Cr17 annealed to achieve spheroidized carbides and turnedFerritischer Edelstahl
DIN 1654-5 Grade X6Cr17 cold drawn, annealed to achieve spheroidized carbides and slightly skin passedMartensitischer Edelstahl
EN 10250-4 Grade X20Cr13 quenched and tempered (+QT)