CEN/TS 13388 Grade CW112C R300, H070

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Durchmesser

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

143 GPa

Show Material materials with Elastic modulus of 143 GPa

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Elongation A100

20.0 °C

20 %

Show Material materials with Elongation A100 of 20 %

Hardness, Brinell

20.0 °C

70 - 100 [-]

Show Material materials with Hardness, Brinell of 70 - 100 [-]

Hardness, Vickers

20.0 °C

75 - 105 [-]

Show Material materials with Hardness, Vickers of 75 - 105 [-]

Tensile strength

20.0 °C

300 MPa

Show Material materials with Tensile strength of 300 MPa

Yield strength Rp0.2

20.0 °C

110 MPa

Show Material materials with Yield strength Rp0.2 of 110 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

100.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

Melting point

1030 - 1050 °C

Show Material materials with Melting point of 1030 - 1050 °C

Specific heat capacity

20.0 °C

399 J/(kg·K)

Show Material materials with Specific heat capacity of 399 J/(kg·K)

Thermal conductivity

20.0 °C

59 - 120 W/(m·K)

Show Material materials with Thermal conductivity of 59 - 120 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

8.00E+6 - 2.30E+7 S/m

Show Material materials with Electrical conductivity of 8.00E+6 - 2.30E+7 S/m

Electrical resistivity

20.0 °C

4.35E-8 - 1.25E-7 Ω·m

Show Material materials with Electrical resistivity of 4.35E-8 - 1.25E-7 Ω·m

Chemical properties

PropertyValue

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Nickel

2.6 - 4.5 %

Show Material materials with Nickel of 2.6 - 4.5 %

Other

Rest Cu, total 0.5

Silicon

0.8 - 1.3 %

Show Material materials with Silicon of 0.8 - 1.3 %

Technological properties

Property
Brazing

soft brazing: good

Workability

general (condition): good