Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Kohlenstoffarmer Stahl
EN 10216-2 Grade P265GH normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10216-2 Grade St 45.8 normalized or normalized formed (+N)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 34CrNiMo6 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10277-5 Grade 30CrMoV9 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 30CrNiMo8 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 cold drawn or turned and quenched and temperedNickel Chromium Molybdenum Steel
EN 10269 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10269 Grade 34CrNiMo6 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 quenched and tempered and cold drawn (+QT+C)Nickel Chromium Molybdenum Steel
EN 10277-5 Grade 34CrNiMo6 cold drawn and quenched and tempered (+C+QT)Chromium Molybdenum Steel
EN 10297-1 Grade 30CrMoV9 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10297-1 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10297-1 Grade 34CrNiMo6 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10263-4 Grade 30CrNiMo8 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10263-4 Grade 34CrNiMo6 quenched and tempered (+QT)