Molybdenum Steel
EN 10028-2 Grade 18MnMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
JIS G3460 Grade STPL380Kohlenstoffarmer Stahl
JIS C2555 Grade PCYH250 hot-rolledKohlenstoffarmer Stahl
JIS C2555 Grade PCYH300 hot-rolledKohlenstoffarmer Stahl
JIS G3456 Grade STPT410Kohlenstoffarmer Stahl
JIS G3461 Grade STB510Kohlenstoffarmer Stahl
JIS G3454 Grade STPG370Kohlenstoffarmer Stahl
JIS G3455 Grade STS370Kohlenstoffarmer Stahl
JIS G3455 Grade STS410Kohlenstoffarmer Stahl
JIS G3455 Grade STS480Kohlenstoffarmer Stahl
JIS G3456 Grade STPT370