General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Elongation | 16.5 % Show Material materials with Elongation of 16.5 % | Predicted Value, A200 | ||||
18.9 % Show Material materials with Elongation of 18.9 % | Predicted Value, Transverse | |||||
19.4 % Show Material materials with Elongation of 19.4 % | Predicted Value, A80 Transverse | |||||
21.6 % Show Material materials with Elongation of 21.6 % | Predicted Value, A50 | |||||
21.9 % Show Material materials with Elongation of 21.9 % | Predicted Value | |||||
24.1 % Show Material materials with Elongation of 24.1 % | Predicted Value, A5 | |||||
20 °C | 19 % Show Material materials with Elongation of 19 % | cold rolled | EN 10326, EN 10346 | Strip | A80 | |
Hardness, Brinell | 240 [-] Show Material materials with Hardness, Brinell of 240 [-] | Predicted Value, Transverse | ||||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel | ||||
Reduction of area | 39.2 % Show Material materials with Reduction of area of 39.2 % | Predicted Value | ||||
43.1 % Show Material materials with Reduction of area of 43.1 % | Predicted Value, Transverse | |||||
Shear modulus | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel | ||||
Shear strength | 499.5 MPa Show Material materials with Shear strength of 499.5 MPa | Predicted Value | ||||
Tensile strength | 20 °C | 330 MPa Show Material materials with Tensile strength of 330 MPa | cold rolled | EN 10326, EN 10346 | Strip |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max service temperature | 310.4 °C Show Material materials with Max service temperature of 310.4 °C | Predicted Value, Long |
500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Specific heat capacity | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 25 - 93 W/(m·K) Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 8 S/m Show Material materials with Electrical conductivity of 8 S/m | Predicted Value |
Electrical resistivity | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % | cold rolled | EN 10326, EN 10346 | Strip |
Manganese | 1.7 % Show Material materials with Manganese of 1.7 % | cold rolled | EN 10326, EN 10346 | Strip |
Phosphorus | 0.1 % Show Material materials with Phosphorus of 0.1 % | cold rolled | EN 10326, EN 10346 | Strip |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % | cold rolled | EN 10326, EN 10346 | Strip |
Sulfur | 0.045 % Show Material materials with Sulfur of 0.045 % | cold rolled | EN 10326, EN 10346 | Strip |