General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Molybdenum Steel | ||||
Elongation | 15.9 % Show Material materials with Elongation of 15.9 % | Predicted Value, A200 | ||||
16.0 % Show Material materials with Elongation of 16.0 % | Predicted Value, A80 | |||||
18.4 % Show Material materials with Elongation of 18.4 % | Predicted Value, A80 Transverse | |||||
19.5 % Show Material materials with Elongation of 19.5 % | Predicted Value, A5 | |||||
20.6 % Show Material materials with Elongation of 20.6 % | Predicted Value, A50 | |||||
20 °C | 20 % Show Material materials with Elongation of 20 % | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse | |
20 °C | 20 % Show Material materials with Elongation of 20 % | quenched and tempered (+QT) | EN 10028-2 | Flat | ||
Hardness, Brinell | 242 [-] Show Material materials with Hardness, Brinell of 242 [-] | Predicted Value, Transverse | ||||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Molybdenum Steel | ||||
Reduction of area | 43.0 % Show Material materials with Reduction of area of 43.0 % | Predicted Value | ||||
44.8 % Show Material materials with Reduction of area of 44.8 % | Predicted Value, Transverse | |||||
Shear modulus | 79.5 GPa Show Material materials with Shear modulus of 79.5 GPa | Predicted Value | ||||
Shear strength | 691.1 MPa Show Material materials with Shear strength of 691.1 MPa | Predicted Value | ||||
Tensile strength | 20 °C | 480 - 620 MPa Show Material materials with Tensile strength of 480 - 620 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse |
20 °C | 480 - 620 MPa Show Material materials with Tensile strength of 480 - 620 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat |
Thermal
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.29e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.29e-05 1/K | Typical for Molybdenum Steel | |||
Max service temperature | 20 - 450 °C Show Material materials with Max service temperature of 20 - 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long |
450 °C Show Material materials with Max service temperature of 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long | |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Molybdenum Steel | |||
Specific heat capacity | 456 J/(kg·K) Show Material materials with Specific heat capacity of 456 J/(kg·K) | Typical for Molybdenum Steel | |||
Thermal conductivity | 37 - 48 W/(m·K) Show Material materials with Thermal conductivity of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Copper | 0.3 % Show Material materials with Copper of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Manganese | 0.9 - 1.5 % Show Material materials with Manganese of 0.9 - 1.5 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Molybdenum | 0.45 - 0.6 % Show Material materials with Molybdenum of 0.45 - 0.6 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Nitrogen | 0.012 % Show Material materials with Nitrogen of 0.012 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Phosphorus | 0.015 % Show Material materials with Phosphorus of 0.015 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Sulfur | 0.005 % Show Material materials with Sulfur of 0.005 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
0.01 % Show Material materials with Sulfur of 0.01 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |