Kohlenstoffarmer Stahl
EN 10149-3 Grade S260NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-3 Grade S355NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P265NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Ferritischer Edelstahl
EN 10088-1 Grade X2CrTi17 soft annealed (+A)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoCuN25-6-3 solution annealed (+AT)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiN23-4 solution annealed (+AT)Ferritischer Edelstahl
EN 10028-7 Grade X2CrTi17 soft annealed (+A)Kohlenstoffarmer Stahl
EN 10268 Grade H280LA skin passedKohlenstoffarmer Stahl
EN 10139 Grade DC04 cold-rolled, strain-hardened (C290)Kohlenstoffarmer Stahl
EN 10139 Grade DC01 cold rolled, skin passedKohlenstoffarmer Stahl
EN 10139 Grade St 4 cold rolled, skin passed (K32)