General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.18 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.18 [-] | max. |
Dimension
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 20 °C | 27 J Show Supplier Material materials with Charpy impact energy of 27 J | min. | for thickness 1.5-20 mm |
Elongation | 23 % Show Supplier Material materials with Elongation of 23 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
24 % Show Supplier Material materials with Elongation of 24 % | min. | for thickness 2-3 mm | Transverse, A80 | ||
28 % Show Supplier Material materials with Elongation of 28 % | min. A5.65√So | for thickness 3-20 mm | ||
Tensile strength | 360 - 430 MPa Show Supplier Material materials with Tensile strength of 360 - 430 MPa | for thickness 1.5-20 mm | Transverse | |
Yield strength | 240 - 360 MPa Show Supplier Material materials with Yield strength of 240 - 360 MPa | for thickness 1.5-2 mm | Transverse | |
240 - 340 MPa Show Supplier Material materials with Yield strength of 240 - 340 MPa | for thickness 2-20 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 % Show Supplier Material materials with Aluminium of 0.01 % | min. |
Carbon | 0.02 - 0.12 % Show Supplier Material materials with Carbon of 0.02 - 0.12 % | |
Manganese | 0.6 % Show Supplier Material materials with Manganese of 0.6 % | max. |
Phosphorus | 0.03 % Show Supplier Material materials with Phosphorus of 0.03 % | max. |
Silicon | 0.03 % Show Supplier Material materials with Silicon of 0.03 % | max. |
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural forming grade which is well suited to applications requiring high reproducibility of processing performance (especially control of springback). The S240D AM FCE grade is popular with Steel Service Centres, since it allows them to rationalise their supplies of deep drawable and structural steel. This grade is a versatile material for numerous applications in industry markets. | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |