Kohlenstoffarmer Stahl
EN 10149-3 Grade S355NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Ferritischer Edelstahl
EN 10088-1 Grade X6CrMoNb17-1 soft annealed (+A)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoCuN25-6-3 solution annealed (+AT)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoCuWN25-7-4 solution annealed (+AT)Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiN23-4 solution annealed (+AT)Ferritischer Edelstahl
EN 10088-4 Grade X2CrTi12 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrAlTi18-2 soft annealed (+A)Ferritischer Edelstahl
EN 10095 Grade X3CrAlTi18-2 soft annealed (+A)Ferritischer Edelstahl
SEW 470 Grade X3CrAlTi18-2 soft annealed (+A)Kohlenstoffarmer Stahl
EN 10111 Grade StW 22 hot rolledKohlenstoffarmer Stahl
EN 10139 Grade DC01 cold rolled, skin passedKohlenstoffarmer Stahl
JIS G3131 Grade HR2Kohlenstoffarmer Stahl
JIS G3313 Grade HR2