Flexural yield strength: 210 MPa

Quick Comparison

Polyamide 46 (PA46)

Stanyl® HFX61S

Geliefert von:

DSM Engineering Materials

Polybutylenterephthalat (PBT)

Arnite® TV4 261

Geliefert von:

DSM Engineering Materials

Polybutylenterephthalat (PBT)

VALOX™ Resin 4031

Polyamide 66 (PA66)

Akulon® S223-HG7

Geliefert von:

DSM Engineering Materials

Polymermischung (Blend)

VALOX™ Resin 8032UX

Polyphthalamid (PPA)

ForTii® MX3

Geliefert von:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

Xytron™ G3010E

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-G7

Geliefert von:

DSM Engineering Materials