General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.1 GPa Show Supplier Material materials with Elastic modulus of 4.1 GPa | conditioned | ISO 527-1/-2 | |
8.2 GPa Show Supplier Material materials with Elastic modulus of 8.2 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | dry | ISO 527-1/-2 | |
200 °C | 1.8 GPa Show Supplier Material materials with Elastic modulus of 1.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | dry | ISO 527-1/-2 | |
15 % Show Supplier Material materials with Elongation of 15 % | conditioned | ISO 527-1/-2 | ||
120 °C | 11 % Show Supplier Material materials with Elongation of 11 % | dry | ISO 527-1/-2 | |
160 °C | 11 % Show Supplier Material materials with Elongation of 11 % | dry | ISO 527-1/-2 | |
200 °C | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 | |
Flexural modulus | 3.3 GPa Show Supplier Material materials with Flexural modulus of 3.3 GPa | conditioned | ISO 178 | |
6.7 GPa Show Supplier Material materials with Flexural modulus of 6.7 GPa | dry | ISO 178 | ||
Flexural yield strength | 95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | conditioned | ISO 178 | |
210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | dry | ISO 179/1eA | |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 73 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 73 kJ/m² | dry | ISO 179/1eU | |
23 °C | 77 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 77 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 62 MPa Show Supplier Material materials with Tensile strength of 62 MPa | conditioned | ISO 527-1/-2 | |
145 MPa Show Supplier Material materials with Tensile strength of 145 MPa | dry | ISO 527-1/-2 | ||
120 °C | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | dry | ISO 527-1/-2 | |
160 °C | 53 MPa Show Supplier Material materials with Tensile strength of 53 MPa | dry | ISO 527-1/-2 | |
200 °C | 38 MPa Show Supplier Material materials with Tensile strength of 38 MPa | dry | ISO 527-1/-2 |
Thermal
Technological properties
Property | ||
---|---|---|
Fillers | 25% Glass Fiber |