Flexural yield strength: 55 MPa

Quick Comparison

Polyamide 6 (PA6)

Akulon® K222-KMV5

Geliefert von:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

Xytron™ G3010E

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K222-KMV5 /A

Geliefert von:

DSM Engineering Materials

Polybutylenterephthalat (PBT)

Arnite® TV4 230

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® SafeConnect SC21

Geliefert von:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

Xytron™ G3080E

Geliefert von:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q210E-H

Geliefert von:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q150-D

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K240-HPG3

Geliefert von:

DSM Engineering Materials