General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Density | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | dry | ISO 1183 |
Limiting oxygen index | 24 % Show Supplier Material materials with Limiting oxygen index of 24 % | dry | ISO 4589-1/-2 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Water absorption | 5.8 % Show Supplier Material materials with Water absorption of 5.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 3.1 GPa Show Supplier Material materials with Elastic modulus of 3.1 GPa | dry | ISO 527-1/-2 |
1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | conditioned | ISO 527-1/-2 | ||
3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.6 GPa Show Supplier Material materials with Elastic modulus of 0.6 GPa | dry | ISO 527-1/-2 | |
140 °C | 0.46 GPa Show Supplier Material materials with Elastic modulus of 0.46 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 |
20 % Show Supplier Material materials with Elongation of 20 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | -40 °C | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 |
4.4 % Show Supplier Material materials with Elongation at yield of 4.4 % | dry | ISO 527-1/-2 | ||
15 % Show Supplier Material materials with Elongation at yield of 15 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 1.4 GPa Show Supplier Material materials with Flexural modulus of 1.4 GPa | conditioned | ISO 178 | |
2.9 GPa Show Supplier Material materials with Flexural modulus of 2.9 GPa | dry | ISO 178 | ||
Flexural yield strength | 55.0 MPa Show Supplier Material materials with Flexural yield strength of 55.0 MPa | conditioned | ISO 178 | |
115 MPa Show Supplier Material materials with Flexural yield strength of 115 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | conditioned | ISO 179/1eA | |
Tensile strength | -40 °C | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | dry | ISO 527-1/-2 |
40 MPa Show Supplier Material materials with Tensile strength of 40 MPa | conditioned | ISO 527-1/-2 | ||
55.0 MPa Show Supplier Material materials with Tensile strength of 55.0 MPa | dry | ISO 527-1/-2 | ||
120 °C | 40 MPa Show Supplier Material materials with Tensile strength of 40 MPa | dry | ISO 527-1/-2 | |
140 °C | 35 MPa Show Supplier Material materials with Tensile strength of 35 MPa | dry | ISO 527-1/-2 | |
Yield strength | -40 °C | 115 MPa Show Supplier Material materials with Yield strength of 115 MPa | dry | ISO 527-1/-2 |
55.0 MPa Show Supplier Material materials with Yield strength of 55.0 MPa | conditioned | ISO 527-1/-2 | ||
85 MPa Show Supplier Material materials with Yield strength of 85 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 77 °C Show Supplier Material materials with Heat deflection temperature of 77 °C | dry | ISO 75-1/-2 | 2 MPa | |
175 °C Show Supplier Material materials with Heat deflection temperature of 175 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 280 °C | 8 g/10min Show Supplier Material materials with Melt mass-flow rate of 8 g/10min | dry | ISO 1133 | |
Melt volume-flow rate | 280 °C | 8.5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 8.5 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | ISO 294-4 | Normal | |
2.4 % Show Supplier Material materials with Shrinkage of 2.4 % | dry | ISO 294-4 | Parallel | ||
Viscosity number | 210 cm³/gr Show Supplier Material materials with Viscosity number of 210 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Abrasive brush monofilament | |
Certifications | Yellow Card Available |