Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-5 Grade S355J2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-5 Grade S355K2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Austenitischer rostfreier Stahl
ASTM A276 Grade S20910 AnnealedWrought Copper Bronze Aluminium Bronze
NC4 - CuAl10Ni5Fe4 - C63000 / C63200Geliefert von:
Lebronze AlloysFerritischer Edelstahl
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Nickel Chromium Alloy
DIN 17742 Grade NiCr15Fe soft annealed (+A)Wrought Copper Nickel Grade
NIBRON SPECIAL® Copper AlloyWrought Copper High Copper Alloy
EN 1652 Grade CuCo2Be THFerritischer Edelstahl
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10277-4 Grade C15R soft annealed and cold drawn (+A+C)Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 TH