DECLAFOR 1015 TH1 - CuNi7.5Sn5Te

Want to keep this datasheet? Save it now in your required format

Description

Connectivity and free-machining alloy.


Spinodal hardening, ageable alloy with outstanding strength and thermal stress relaxation properties.

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.8 g/cm³

Show Supplier Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Available size round products (mm): 1-14

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

115 GPa

Show Supplier Material materials with Elastic modulus of 115 GPa

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

Hardness, Brinell

23.0 °C

223 - 271 [-]

Show Supplier Material materials with Hardness, Brinell of 223 - 271 [-]

Hardness, Rockwell C

23.0 °C

20 - 29 [-]

Show Supplier Material materials with Hardness, Rockwell C of 20 - 29 [-]

Hardness, Vickers

23.0 °C

230 - 280 [-]

Show Supplier Material materials with Hardness, Vickers of 230 - 280 [-]

Tensile strength

23.0 °C

780 - 840 MPa

Show Supplier Material materials with Tensile strength of 780 - 840 MPa

Yield strength

23.0 °C

550 - 750 MPa

Show Supplier Material materials with Yield strength of 550 - 750 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.72E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.72E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

55 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 55 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

8.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 8.00E+6 S/m

Technological properties

Property
Application areas

Summary of typical applications: Connectors, precision mechanical & electrical parts

Corrosion properties

Corrosion resistance rating: 4 out of 5

General machinability

Machinability: 60 %

Processing history

Condition: TH1