Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1200-2 austemperedWrought Copper High Copper Alloy
EN 12166 Grade CuBe2Pb H350Wrought Copper High Copper Alloy
EN 12165 Grade CuBe2 MChromium Molybdenum Steel
DIN 1.7734 6Wrought Copper High Copper Alloy
EN 12163 Grade CuBe2 MHartstahl
ASTM A551 Class DHT Heat-TreatedWrought Copper High Copper Alloy
EN 12163 Grade CuBe2 H350Wrought Copper High Copper Alloy
EN 12166 Grade CuBe2 H350Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 H340Wrought Copper High Copper Alloy
EN 12163 Grade CuBe2 F00Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1400-1 cast conditionMartensitischer Edelstahl
ASTM A693 Grade XM-12 Solution-TreatedMartensitischer Edelstahl
ASTM A705 Grade XM-12 Solution Annealed