Heat deflection temperature, 1.80 MPa: 74 °C

Quick Comparison

Polyphenylether (PPE)

NORYL™ Resin RN0612 - Europe

Geliefert von:

Sabic

Polymermischung (Blend)

LNP™ STAT-LOY™ Compound 63000CTU

Geliefert von:

Sabic

Polypropylen (PP)

LNP™ STAT-KON™ Compound MX18001J

Geliefert von:

Sabic

Polyamide 66 (PA66)

Zytel® FG53 NC010

Polyphenylether (PPE)

NORYL™ Resin FP3060 - Europe

Geliefert von:

Sabic

Polyamide 66 (PA66)

Zytel® FG50 NC010

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RL002 - Americas

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RL002 - Europe

Geliefert von:

Sabic