General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.16 g/cm³ Show Supplier Material materials with Density of 1.16 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1.2 GPa Show Supplier Material materials with Elastic modulus of 1.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 200 % Show Supplier Material materials with Elongation of 200 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 1.2 GPa Show Supplier Material materials with Flexural modulus of 1.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 53 MPa Show Supplier Material materials with Flexural strength of 53 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Charpy notched | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 69 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Izod notched | 23.0 °C | 500 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 500 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 500 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 500 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 36 MPa Show Supplier Material materials with Tensile strength of 36 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 74 - 83 °C Show Supplier Material materials with Heat deflection temperature of 74 - 83 °C | |
Heat deflection temperature, 0.45 MPa | 83 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 83 °C | ASTM D 648 | 6.4 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 74 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 74 °C | ASTM D 648 | 6.4 mm, unannealed |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+11 - 5.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+11 - 5.00E+12 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+11 - 5.00E+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+11 - 5.00E+12 Ω·cm | ASTM D 257 |
Optical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 19 g/10min Show Supplier Material materials with Melt mass-flow rate of 19 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | SABIC method |
Shrinkage, transverse | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage, transverse of 0.6 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor, Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |