NORYL™ Resin FP3060 - Europe

Want to keep this datasheet? Save it now in your required format

Description

NORYL™ FP3060 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant with a UL94 flame rating of V0 at 2.5mm and V0 at 2.5mm. NORYL FP3060 resin was designed to have very good dimensional stability with high flow and exhibits good rheological properties, high heat resistance, hydrolysis resistance, and very low density. The combination of these properties makes this material an excellent candidate for Flat Panel TV enclosure applications.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.1 g/cm³

Show Supplier Material materials with Density of 1.1 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.02 %

Show Supplier Material materials with Moisture absorption of 0.02 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.1 [-]

Show Supplier Material materials with Relative density of 1.1 [-]

ASTM D 792 |

Water absorption

23.0 °C

0.13 %

Show Supplier Material materials with Water absorption of 0.13 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.42 GPa

Show Supplier Material materials with Elastic modulus of 2.42 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ISO 527 | yield, 50 mm/min

Flexural modulus

23.0 °C

2.53 GPa

Show Supplier Material materials with Flexural modulus of 2.53 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

82 MPa

Show Supplier Material materials with Flexural strength of 82 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m²

ISO 180/1A | 80*10*4, -30°C

Impact strength, Izod notched, ASTM

23.0 °C

78 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 78 J/m

ASTM D 256 | notched, 23°C

Tensile strength

23.0 °C

42 MPa

Show Supplier Material materials with Tensile strength of 42 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8.3E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8.3E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature

74 °C

Show Supplier Material materials with Heat deflection temperature of 74 °C

Heat deflection temperature, 1.80 MPa

74 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 74 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

UL 746B

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

UL 746B

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

UL 746B

Vicat softening temperature

91 °C

Show Supplier Material materials with Vicat softening temperature of 91 °C

ISO 306 | Rate B/50

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100064745- -

Rheological Properties

PropertyValueComment

Melt mass-flow rate

42 g/10min

Show Supplier Material materials with Melt mass-flow rate of 42 g/10min

ASTM D 1238 | 200°C/3.8 kgf

Melt volume-flow rate

20 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min

ISO 1133 | MVR at 280°C/1.2 kg

Technological properties

Property
Application areas

Displays, Medical Device

Availability

Europe

Features

Low Creep Sensitivity, Flame Retardant, Non-Halogenated, Non-Chlorinated, Non-Brominated, High Flow

Processing methods

Hopper Temperature: 60 to 80.0°C
Front - Zone 3 Temperature: 250 to 285.0°C
Rear - Zone 1 Temperature: 200 to 220.0°C
Drying Temperature: 65 to 75.0°C
Melt Temperature: 250 to 285.0°C
Middle - Zone 2 Temperature: 230 to 260.0°C
Mold Temperature: 40 to 65.0°C
Nozzle Temperature: 240 to 270.0°C
Drying Time: 2 to 3.0hrs

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.