Impact strength, Izod unnotched, ASTM: 410 J/m

Quick Comparison

Polyetherimid (PEI)

ULTEM™ Resin 2410EPR - Europe

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2410EPR - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2410EPR - Americas

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin GFN1F - Asia

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ STAT-KON™ Compound DX13320C

Geliefert von:

Sabic

Polypropylen (PP)

SABIC® PPcompound 1920

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DEL34E

Geliefert von: