General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Density of 1.38 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | ASTM D 638 | 50 mm/min |
Flexural modulus | 23.0 °C | 12.5 GPa Show Supplier Material materials with Flexural modulus of 12.5 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 214 MPa Show Supplier Material materials with Flexural strength of 214 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 86 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 86 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 86 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 86 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 410 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 410 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 152 MPa Show Supplier Material materials with Tensile strength of 152 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 137 - 143 °C Show Supplier Material materials with Heat deflection temperature of 137 - 143 °C | |
Heat deflection temperature, 0.45 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 143 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Document Handling, Enclosures | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |