Instrumented Impact, Total Energy: 11 J

Quick Comparison

Polymermischung (Blend)

LNP™ LUBRICOMP™ Compound OFL36XXC

Geliefert von:

Sabic

Polymermischung (Blend)

LNP™ FARADEX™ Compound NX07344

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ LUBRICOMP™ Compound ECL36XXQ

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ STAT-KON™ Compound EEF42

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF203AXH

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DC006ERH

Geliefert von:

Sabic

Acrylnitril-Butadien-Styrol (ABS)

LNP™ THERMOCOMP™ Compound AF004L

Geliefert von:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOTUF™ Compound PX95726

Geliefert von:

Sabic

Polyethersulfon (PES)

LNP™ THERMOCOMP™ Compound JF004L

Geliefert von:

Sabic

Polypropylen (PP)

LNP™ THERMOCOMP™ Compound MC002

Geliefert von:

Sabic

Acrylnitril-Butadien-Styrol (ABS)

LNP™ THERMOCOMP™ Compound AF004AH

Geliefert von:

Sabic