General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.36 g/cm³ Show Supplier Material materials with Density of 1.36 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.28 % Show Supplier Material materials with Moisture absorption of 0.28 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.36 [-] Show Supplier Material materials with Relative density of 1.36 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 8.9 GPa Show Supplier Material materials with Flexural modulus of 8.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 214 MPa Show Supplier Material materials with Flexural strength of 214 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 56 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 56 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 38 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 38 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 632 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 632 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 11 J Show Supplier Material materials with Instrumented Impact, Total Energy of 11 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 141 MPa Show Supplier Material materials with Tensile strength of 141 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.5E-5 1/K | ASTM D 696 | -30°C to 30°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 4.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.4E-5 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature | 137 - 144 °C Show Supplier Material materials with Heat deflection temperature of 137 - 144 °C | ||
Heat deflection temperature, 0.45 MPa | 144 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 144 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |