Austenitischer rostfreier Stahl
Alloy 24 / 1.4565 Solution annealed and quenchedGeliefert von:
Hempel Special MetalsDuplex rostfreier Stahl
Sandvik SAF 2707 HD™Geliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
ASTM A276 Grade S20910 AnnealedAustenitischer rostfreier Stahl
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Austenitischer rostfreier Stahl
EN 10095 Grade X25CrMnNiN25-9-7 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X55CrMnNiN20-8 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
ASTM A213 Grade XM-19 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A688 Grade TPXM-29 Solution-AnnealedAustenitischer rostfreier Stahl
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
ASTM A193 Grade B8R Class 1C, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8R Class 1D, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8RA Class 1C, Carbide solution treated in the finished conditionAustenitischer rostfreier Stahl
ASTM A213 Grade S34565 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade XM-19 Heat-Treated