Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J0C as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P245NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P265NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P310NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P355NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
DIN 1629 Grade St 37.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1629 Grade St 44.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1626 Grade USt 37.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG2C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235J0C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S275J0C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S275JRC as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG1 as-rolled condition (+AR)