EN 10025-2 Grade S355J0C as-rolled condition (+AR)

View all suppliers (3)

Want to keep this datasheet? Save it now in your required format

Description

S355J0C is used for folding, section cold forming and cold drawing grade. The high-tensile fine grained steel is applicable for welding constructions up to -20 °C subject to the load. Compared to S235J0C is achievable a considerable saving of material due to the by 120 MPa higher yield point. The steel shows a by 15% higher resistance to mineral wear due to sliding action in comparison to S235J0. Max. product thickness amounts 20 mm for folding and 8 mm for cold roll forming grades.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation

17.1 %

Show Material materials with Elongation of 17.1 %

Predicted Value, A200

21.8 %

Show Material materials with Elongation of 21.8 %

Predicted Value, A5

23.2 %

Show Material materials with Elongation of 23.2 %

Predicted Value, A50

20 °C

12 %

Show Material materials with Elongation of 12 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80 Transverse

20 °C

13 %

Show Material materials with Elongation of 13 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80 Transverse

20 °C

14 %

Show Material materials with Elongation of 14 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80 Transverse

20 °C

15 %

Show Material materials with Elongation of 15 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80 Transverse

20 °C

16 %

Show Material materials with Elongation of 16 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80 Transverse

20 °C

16 %

Show Material materials with Elongation of 16 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80

20 °C

17 %

Show Material materials with Elongation of 17 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80

20 °C

18 %

Show Material materials with Elongation of 18 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

A80

20 °C

20 %

Show Material materials with Elongation of 20 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Flat, Bar, Sheet, Strip

Transverse

20 °C

22 %

Show Material materials with Elongation of 22 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Flat, Bar, Sheet, Strip

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Reduction of area

41.0 %

Show Material materials with Reduction of area of 41.0 %

Predicted Value

43.7 %

Show Material materials with Reduction of area of 43.7 %

Predicted Value, Transverse

Shear modulus

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Shear strength

513.2 MPa

Show Material materials with Shear strength of 513.2 MPa

Predicted Value

Tensile strength

20 °C

490 - 630 MPa

Show Material materials with Tensile strength of 490 - 630 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

20 °C

490 - 680 MPa

Show Material materials with Tensile strength of 490 - 680 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

20 °C

510 - 680 MPa

Show Material materials with Tensile strength of 510 - 680 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

20 °C

510 - 630 MPa

Show Material materials with Tensile strength of 510 - 630 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Sheet, Strip, Flat

Yield strength

254.2 MPa

Show Material materials with Yield strength of 254.2 MPa

Predicted Value, RP1

316.5 MPa

Show Material materials with Yield strength of 316.5 MPa

Predicted Value, RP1 Transverse

350.6 MPa

Show Material materials with Yield strength of 350.6 MPa

Predicted Value, Transverse

355.9 MPa

Show Material materials with Yield strength of 355.9 MPa

Predicted Value, RP02

366.5 MPa

Show Material materials with Yield strength of 366.5 MPa

Predicted Value, RP05

446.5 MPa

Show Material materials with Yield strength of 446.5 MPa

Predicted Value, RP02 Transverse

482.8 MPa

Show Material materials with Yield strength of 482.8 MPa

Predicted Value, RP002

20 °C

345 MPa

Show Material materials with Yield strength of 345 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

20 °C

355 MPa

Show Material materials with Yield strength of 355 MPa

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

1.32e-05 - 1.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K

Typical for Low Carbon Steel

Max service temperature

-20 °C

Show Material materials with Max service temperature of -20 °C

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Long

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

Typical for Low Carbon Steel

Thermal conductivity

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

Typical for Low Carbon Steel

Electrical

PropertyValueComment

Electrical conductivity

8 S/m

Show Material materials with Electrical conductivity of 8 S/m

Predicted Value

Electrical resistivity

1.43e-07 - 1.74e-07 Ω·m

Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValueConditionRelated StandardsShape

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Manganese

1.6 %

Show Material materials with Manganese of 1.6 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Nitrogen

0.009 %

Show Material materials with Nitrogen of 0.009 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Silicon

0.55 %

Show Material materials with Silicon of 0.55 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Sulfur

0.04 %

Show Material materials with Sulfur of 0.04 %

as-rolled condition (+AR)

EN 10025, EN 10025-1, EN 10025-2

Bar, Sheet, Strip, Flat

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.