Zugfestigkeit: 80 - 90 MPa

Quick Comparison

Polycarbonat (PC)

LEXAN™ Copolymer DMX9455A

Geliefert von:

Sabic

Polyamide 46 (PA46)

Stanyl® 46HF5040

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE250F8

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 101 NC010

Polyamide 46 (PA46)

Stanyl® TW200F6

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F6

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6-FC

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6

Geliefert von:

DSM Engineering Materials

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound D151

Geliefert von:

Sabic

Polyamide 4T (PA4T)

ForTii® F11

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS250F8

Geliefert von:

DSM Engineering Materials

Polyetherimid (PEI)

ULTEM™ Resin MD130 - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin MD131 - Europe

Geliefert von:

Sabic

1000 Series

EN 573-3 Grade AW-1050A O

Geliefert von:

2 Matmatch-Lieferanten

1000 Series

EN 573-3 Grade AW-1050A O

Geliefert von:

2 Matmatch-Lieferanten

5000 Serie

EN 573-3 Grade AW-5005 O

Geliefert von:

1 Matmatch-Lieferant

5000 Serie

EN 573-3 Grade AW-5005 O

Geliefert von:

1 Matmatch-Lieferant

5000 Serie

EN 573-3 Grade AW-5052 O

Geliefert von:

1 Matmatch-Lieferant

1000 Series

EN 573-3 Grade AW-1050A H111

Geliefert von:

2 Matmatch-Lieferanten

1000 Series

EN 573-3 Grade AW-1070A H111

Geliefert von:

2 Matmatch-Lieferanten