Austenitischer rostfreier Stahl
Esshete 1250Geliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro 31HTGeliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
Sandvik 2RE10Geliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
Sandvik 6R35Geliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro 30 AnnealedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
Sandvik 8R40Geliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
Sandvik 6R44Geliefert von:
Alleima (formerly Sandvik Materials Technology)Grey Cast Iron
EN 1561 Grade GJL-250 cast conditionGrey Cast Iron
EN 1561 Grade GJL-300 cast condition