2000 Serie
EN 573-3 Grade AW-2014 T6522000 Serie
EN 573-3 Grade AW-2014 T6527000 Serie
WL 3.4384 Grade 3.4384 T73517000 Serie
WL 3.4394 Grade 3.4394 T747000 Serie
WL 3.4394 Grade 3.4394 T74517000 Serie
WL 3.4394 Grade 3.4394 T7452Kohlenstoffarmer Stahl
ASTM A871 Type I Grade 60 As-Rolled, Normalized or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A871 Type II Grade 60 As-Rolled, Normalized or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A871 Type II Grade 65 As-Rolled, Normalized or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A765 Grade IV Normalized and Tempered, Double Normalized and Tempered, or Quenched and TemperedKohlenstoffarmer Stahl
ASTM A372 Grade F Class 55, Normalized, Normalized and Tempered, Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and TemperKohlenstoffarmer Stahl
ASTM A694 Grade F56 Normalized, Normalized and Tempered, Quenched and Tempered, or Precipitation HardenedKohlenstoffarmer Stahl
ASTM A694 Grade F60 Normalized, Normalized and Tempered, Quenched and Tempered, or Precipitation HardenedKohlenstoffarmer Stahl
ASTM A694 Grade F65 Normalized, Normalized and Tempered, Quenched and Tempered, or Precipitation HardenedKohlenstoffarmer Stahl
ASTM A694 Grade F70 Normalized, Normalized and Tempered, Quenched and Tempered, or Precipitation HardenedKohlenstoffarmer Stahl
ASTM A694 Grade F50 Normalized, Normalized and Tempered, Quenched and Tempered, or Precipitation HardenedAustenitischer rostfreier Stahl
ASTM A193 Grade B8 Class 2, Carbide solution treated and strain hardened; M20 and underAustenitischer rostfreier Stahl
ASTM A193 Grade B8C Class 2, Carbide solution treated and strain hardened; M20 and underAustenitischer rostfreier Stahl
ASTM A193 Grade B8P Class 2, Carbide solution treated and strain hardened; M20 and underAustenitischer rostfreier Stahl
ASTM A193 Grade B8R Class 1C, Carbide solution treated