Martensitischer Edelstahl
SEW 555 Grade X12CrMoWVNbN10-1-1 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10088-1 Grade X29CrS13 quenched and tempered (+QT850)Nickel Chromium Steel
SEW 555 Grade 27NiCrMoV11-6 quenched and tempered (+QT)Aushärtbarer Stahl
ASTM A564 Grade XM-25 H1100