Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn40 R340Reines Titan
DIN 17850 Grade Ti1Pd AnnealedAustenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10272 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Leaded Brass
EN 1652 Grade CuZn39Pb0.5 R340Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiMo17-13 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNi23-13 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNi25-20 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X6CrNiTi18-10 solution annealed (+AT)Leaded Brass
EN 12166 Grade CuZn40Pb2 H075