General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 4.505 g/cm³ Show Material materials with Density of 4.505 g/cm³ | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 108.0 GPa Show Material materials with Elastic modulus of 108.0 GPa | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | |
200.0 °C | 95.0 GPa Show Material materials with Elastic modulus of 95.0 GPa | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | ||
400.0 °C | 82.0 GPa Show Material materials with Elastic modulus of 82.0 GPa | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | ||
Elongation | 20.0 °C | 24.0 % Show Material materials with Elongation of 24.0 % | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod | Transverse |
20.0 °C | 24.0 % Show Material materials with Elongation of 24.0 % | Annealed | WL 3.7024-1, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Sheet | ||
20.0 °C | 30.0 % Show Material materials with Elongation of 30.0 % | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Welded Tube, Wire | ||
Hardness, Brinell | 20.0 °C | 120.0 Show Material materials with Hardness, Brinell of 120.0 | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod | |
20.0 °C | 120.0 Show Material materials with Hardness, Brinell of 120.0 | Annealed | DIN 17864, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17860 | Forging | Transverse | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | ||||
Reduction of area | 20.0 °C | 35.0 % Show Material materials with Reduction of area of 35.0 % | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod | Transverse |
20.0 °C | 35.0 % Show Material materials with Reduction of area of 35.0 % | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod | ||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | ||||
Tensile strength | 20.0 °C | 290.0 - 410.0 MPa Show Material materials with Tensile strength of 290.0 - 410.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Welded Tube, Wire | |
20.0 °C | 290.0 - 420.0 MPa Show Material materials with Tensile strength of 290.0 - 420.0 MPa | Annealed | WL 3.7024-1, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Sheet | ||
20.0 °C | 290.0 - 410.0 MPa Show Material materials with Tensile strength of 290.0 - 410.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod | Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Tensile strength of 350.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | |||
100.0 °C | 280.0 MPa Show Material materials with Tensile strength of 280.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | |||
200.0 °C | 175.0 MPa Show Material materials with Tensile strength of 175.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | |||
300.0 °C | 140.0 MPa Show Material materials with Tensile strength of 140.0 MPa | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||||
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | ||||
Specific heat capacity | 20.0 °C | 520.0 J/(kg·K) Show Material materials with Specific heat capacity of 520.0 J/(kg·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | |
200.0 °C | 570.0 J/(kg·K) Show Material materials with Specific heat capacity of 570.0 J/(kg·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | ||
400.0 °C | 630.0 J/(kg·K) Show Material materials with Specific heat capacity of 630.0 J/(kg·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | ||
Thermal conductivity | 20.0 °C | 22.6 W/(m·K) Show Material materials with Thermal conductivity of 22.6 W/(m·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | |
200.0 °C | 20.9 W/(m·K) Show Material materials with Thermal conductivity of 20.9 W/(m·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | ||
400.0 °C | 19.3 W/(m·K) Show Material materials with Thermal conductivity of 19.3 W/(m·K) | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical resistivity | 20.0 °C | 4.7e-07 Ω·m Show Material materials with Electrical resistivity of 4.7e-07 Ω·m | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
200.0 °C | 8.2e-07 Ω·m Show Material materials with Electrical resistivity of 8.2e-07 Ω·m | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet | |
400.0 °C | 1.18e-06 Ω·m Show Material materials with Electrical resistivity of 1.18e-06 Ω·m | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.06 Show Material materials with Carbon of 0.06 | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat |
0.08 Show Material materials with Carbon of 0.08 | Annealed | WL 3.7024-1, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Sheet | |
Hydrogen | 0.013 Show Material materials with Hydrogen of 0.013 | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
Iron | 0.15 Show Material materials with Iron of 0.15 | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Welded Tube, Flat, Tube |
0.2 Show Material materials with Iron of 0.2 | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Tube, Sheet | |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Tube, Welded Tube, Flat, Sheet |
Oxygen | 0.12 Show Material materials with Oxygen of 0.12 | Annealed | VdTÜV WB 230-3, WL 3.7024-1, DIN 17850, DIN 17862, DIN 17864, DIN 17860, VdTÜV WB 230-1, VdTÜV WB 230-2 | Forging, Rod, Wire, Welded Tube, Flat, Tube |
0.18 Show Material materials with Oxygen of 0.18 | Annealed | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Tube | |
0.2 Show Material materials with Oxygen of 0.2 | Annealed | WL 3.7024-1, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Sheet | |
Titanium | 98.9 % Show Material materials with Titanium of 98.9 % | Annealed | WL 3.7024-1, DIN 17850, VdTÜV WB 230-1, VdTÜV WB 230-2, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Sheet |
99.1 % Show Material materials with Titanium of 99.1 % | Annealed | DIN 17850, VdTÜV WB 230-2, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Tube | |
99.2 % Show Material materials with Titanium of 99.2 % | Annealed | DIN 17850, VdTÜV WB 230-2, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Welded Tube, Wire, Flat, Tube |