Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.81 g/cm³ Show Material materials with Dichte of 2.81 g/cm³ | T3510 | EN 573-3, EN 754 | Rod, Tube |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 3.0 % Show Material materials with Dehnung of 3.0 % | T3510 | EN 573-3, EN 754 | Rod, Tube | A50 | |
5.0 % Show Material materials with Dehnung of 5.0 % | T3510 | EN 573-3, EN 754 | Rod, Tube | A100 | ||
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | T3510 | EN 573-3 | Rod, Tube | A50 | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T3510 | EN 573-3 | Rod, Tube | ||
Elastizitätsmodul | 72.5 GPa Show Material materials with Elastizitätsmodul of 72.5 GPa | T3510 | EN 573-3, EN 754 | Rod, Tube | ||
Härte, Brinell | 20.0 °C | 115.0 [-] Show Material materials with Härte, Brinell of 115.0 [-] | T3510 | EN 573-3 | Rod, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Schubmodule | 27.2 GPa Show Material materials with Schubmodule of 27.2 GPa | T3510 | EN 573-3, EN 754 | Rod, Tube | ||
Zugfestigkeit | 370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T3510 | EN 573-3, EN 754 | Rod, Tube | ||
20.0 °C | 370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T3510 | EN 573-3 | Rod, Tube |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Schmelzpunkt | 500.0 - 650.0 °C Show Material materials with Schmelzpunkt of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 251.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 6e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bismut | 0.2 % Show Material materials with Bismut of 0.2 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Blei | 0.8 - 1.5 % Show Material materials with Blei of 0.8 - 1.5 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | T3510 | EN 573-3 | Rod, Tube |
0.70 % Show Material materials with Eisen of 0.70 % | T3510 | EN 573-3, EN 754 | Rod, Tube | |
Kupfer | 3.3 - 4.5 % Show Material materials with Kupfer of 3.3 - 4.5 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Magnesium | 0.5 - 1.3 % Show Material materials with Magnesium of 0.5 - 1.3 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Mangan | 0.2 - 1.0 % Show Material materials with Mangan of 0.2 - 1.0 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Zink | 0.5 % Show Material materials with Zink of 0.5 % | T3510 | EN 573-3, EN 754 | Rod, Tube |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |