Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.47 g/cm³ Show Material materials with Dichte of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Schmelzpunkt | 905 - 932 °C Show Material materials with Schmelzpunkt of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass | |
Spezifische Wärmekapazität | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Wärmeleitfähigkeit | 23.0 °C | 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 5 - 6.5 % Show Material materials with Aluminium of 5 - 6.5 % |
Andere | Rest Zn, total 1.0 |
Antimon | 0.01 % Show Material materials with Antimon of 0.01 % |
Arsen | 0.02 % Show Material materials with Arsen of 0.02 % |
Bismut | 1E-3 % Show Material materials with Bismut of 1E-3 % |
Blei | 0.5 % Show Material materials with Blei of 0.5 % |
Eisen | 1 - 2.5 % Show Material materials with Eisen of 1 - 2.5 % |
Kupfer | 61 - 63.5 % Show Material materials with Kupfer of 61 - 63.5 % |
Mangan | 2.5 - 3.5 % Show Material materials with Mangan of 2.5 - 3.5 % |
Nickel | 1 - 2 % Show Material materials with Nickel of 1 - 2 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Silizium | 0.03 % Show Material materials with Silizium of 0.03 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |