Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Härte, Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Härte, Brinell of 120 - 150 [-] |
Härte, Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Härte, Vickers of 125 - 155 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 20.0 °C | 500 MPa Show Material materials with Zugfestigkeit of 500 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.3 - 7.6 % Show Material materials with Aluminium of 6.3 - 7.6 % |
Andere | Rest Cu, total 0.2 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.2 - 0.3 % Show Material materials with Eisen of 0.2 - 0.3 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Silizium | 1.5 - 2.2 % Show Material materials with Silizium of 1.5 - 2.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |