Whatever special alloy you are looking for: We have it. We have a large range of semi-finished metal products with a special focus on rods and tubes made of bronze, special brass and low-alloy copper alloys. You will find some important international manufacturers exclusively from us

Company profile

Headquarters

Erkrath,North Rhine-Westphalia, Germany

Type

Manufacturer and Processor

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

DIN CuAl10Fe

Sheet, Plate, Bar

DIN CuAl10Fe, DIN CC331G, DIN 2.0940, UNS C95200, BS AB1

DIN EN 1982, DIN 1714, BS 1400

DIN CuAl10Fe3Mn2

Sheet, Plate, Bar

DIN CuAl10Fe3Mn2, DIN 2.0936, EN CW306G, UNS C62300, UNS C62500, BS CA103

DIN EN 12163, DIN EN 12167, DIN EN 12420, DIN 17665, BS 2872, BS 2874

DIN CuAl10Ni

Sheet, Plate, Bar

DIN CuAl10Ni, DIN CC333G, DIN 2.0975, UNS95800, UNS C95500, BS AB2, BS 1400

DIN EN 1982, DIN 1714, BS AB2, BS 1400

DIN CuAl10Ni5Fe4

Sheet, Plate, Bar

DIN CuAl10Ni5Fe4, DIN 2.0966, EN CW307G, UNS C63200, UNS C63000, BS CA104

DIN EN 12163, DIN EN 12167, DIN EN 12420, DIN EN 1653, DIN 17665, BS 2872, BS 2874, BS 2875

DIN CuAl11Ni

Sheet, Plate, Bar

DIN CuAl11Ni, DIN CC334G, DIN 2.0980

DIN EN 1982, DIN 1714, BS AB2, BS 1400

DIN CuAl11Ni6Fe5

Sheet, Plate, Bar

DIN CuAl11Ni6Fe5, DIN 2.0978, DIN CW308G

DIN EN 12163, DIN EN 12167, DIN EN 12420, DIN 17665

DIN CuAl7Si2

Sheet, Plate, Bar

DIN CuAl7Si2, DIN CW302G, UNS C64200

DIN EN 12420, DIN EN 12163, DIN EN 12167

DIN CuAl8Fe3

Sheet, Plate, Bar

DIN CuAl8Fe3, DIN 2.0932, DIN CW303G, BS CA106, UNS C61400

DIN EN 12420, DIN EN 1652, DIN EN 1653, DIN 17665, BS 2874, BS 2875

DIN CuAl9Mn2

Sheet, Plate, Bar

DIN CuAl9Mn2, DIN 2.0960

DIN 17665

DIN CuAl9Ni

Sheet, Plate, Bar

DIN CuAl9Ni, DIN CC332G, DIN 2.0970

DIN 1714