Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | in 2″ (51 mm) |
Härte, Brinell | 23.0 °C | 140 [-] Show Supplier Material materials with Härte, Brinell of 140 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Zugfestigkeit | 23.0 °C | 530 MPa Show Supplier Material materials with Zugfestigkeit of 530 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 7.5 - 9.5 % Show Supplier Material materials with Aluminium of 7.5 - 9.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 1.5 - 2.5 % Show Supplier Material materials with Eisen of 1.5 - 2.5 % | ||
Kupfer | Balance, including silver | ||
Mangan | 1 - 2.5 % Show Supplier Material materials with Mangan of 1 - 2.5 % | ||
Nickel | 1.8 - 3 % Show Supplier Material materials with Nickel of 1.8 - 3 % | ||
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship propellers,Bearing overlays,Pumps,Chemical industry,Breaker blocks,Guide grooves |