Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 6.84 g/cm³ Show Supplier Material materials with Dichte of 6.84 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Druckfestigkeit | 23.0 °C | 1608 MPa Show Supplier Material materials with Druckfestigkeit of 1608 MPa | |
Druckfestigkeit, 0,1% | 23.0 °C | 715 MPa Show Supplier Material materials with Druckfestigkeit, 0,1% of 715 MPa | |
Härte, HBW | 23.0 °C | 420 [-] Show Supplier Material materials with Härte, HBW of 420 [-] | HBW 10/3000 |
Härte, Rockwell C | 23.0 °C | 44 [-] Show Supplier Material materials with Härte, Rockwell C of 44 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 33 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 33 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Chemical properties
Property | Value |
---|---|
Kupfer | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Stainless steel drawing dies, forming rolls under great stresses and extreme pressures are the most typical applications for this alloy. |