Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 3.92 g/cm³ Show Supplier Material materials with Dichte of 3.92 g/cm³ | |
Oberflächenrauigkeit | 3.6 μm Show Supplier Material materials with Oberflächenrauigkeit of 3.6 μm | Rz* |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 440 MPa Show Supplier Material materials with Biegefestigkeit of 440 MPa | 4-point bending flexural test |
Druckfestigkeit | 23.0 °C | 2800 MPa Show Supplier Material materials with Druckfestigkeit of 2800 MPa | |
Elastizitätsmodul | 23.0 °C | 380 GPa Show Supplier Material materials with Elastizitätsmodul of 380 GPa | |
Härte, Vickers | 23.0 °C | 1733 [-] Show Supplier Material materials with Härte, Vickers of 1733 [-] | converted from GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4.3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4.3 MPa·√m |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+14 Ω·m |
600.0 °C | 1000000 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1000000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Wear parts for the textile and the machine engineering industry Suitable for high temperatures and corrosive environments, e.g. in laboratories Insulating parts for electronics and electrical engineering | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Ceramic Injection Molding (CIM) |