Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 600 MPa Show Supplier Material materials with Biegefestigkeit of 600 MPa | 4-point bending flexural test |
Druckfestigkeit | 23.0 °C | 2600 MPa Show Supplier Material materials with Druckfestigkeit of 2600 MPa | |
Elastizitätsmodul | 23.0 °C | 360 GPa Show Supplier Material materials with Elastizitätsmodul of 360 GPa | |
Härte, Vickers | 23.0 °C | 1733 [-] Show Supplier Material materials with Härte, Vickers of 1733 [-] | converted from GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 5 MPa·√m |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 25 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+14 Ω·m |
600.0 °C | 1000000 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1000000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting materials for machine Valves, gear wheels Sensors For highest mechanical loads | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Ceramic Injection Molding (CIM) |