Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 140 MPa Show Supplier Material materials with Biegefestigkeit of 140 MPa | 4-point bending flexural test |
Druckfestigkeit | 23.0 °C | 900 MPa Show Supplier Material materials with Druckfestigkeit of 900 MPa | |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa | |
Härte, Vickers | 23.0 °C | 510 [-] Show Supplier Material materials with Härte, Vickers of 510 [-] | converted from GPa |
Thermisch
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.00E+11 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+11 Ω·m |
600.0 °C | 100000 Ω·m Show Supplier Material materials with spezifischer Widerstand of 100000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Isolators and fuses High frequency technology Especially used in the electronics and automotive industry | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Axial Pressing |